{"paper":{"title":"Generation of silicone poly-HIPES with controlled pore sizes via reactive emulsion stabilization","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.soft","authors_text":"Ana\\\"is Giustiniani, Christophe Poulard, Manon Marchand, Philippe Gu\\'egan, Wiebke Drenckhan","submitted_at":"2016-10-20T08:40:19Z","abstract_excerpt":"Macrocellular silicone polymers are obtained after solidification of the continuous phase of a PDMS (polydimethylsiloxane) emulsion, which contains PEG (polyethylene glycol) drops of sub-millimetric dimensions. Coalescence of the liquid template emulsion is prohibited by a reactive blending approach. We investigate in detail the relationship between the interfacial properties and the emulsion stability, and we use micro- and millifluidic techniques to generation macro-cellular polymers with controlled structural properties over a wider range of cell-sizes (0.2-2mm) and volume fractions of the "},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1610.06327","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}