{"paper":{"title":"Ultra-smooth single crystal diamond surfaces resulting from implantation and lift-off processes","license":"http://arxiv.org/licenses/nonexclusive-distrib/1.0/","headline":"","cross_cats":[],"primary_cat":"cond-mat.mtrl-sci","authors_text":"A. Perrat-Mabilon, B. Fernandez, C. Peaucelle, D. Eon, E. Bustarret, E. Gheeraert, J. Hartwig, P. Olivero, T. A. Lafford, T. N. Tran Thi","submitted_at":"2016-08-25T14:30:18Z","abstract_excerpt":"A method for obtaining a smooth, single crystal diamond surface is presented, whereby a sacrificial defective layer is created by implantation and graphitized by annealing before being selectively etched. We have used O+ at 240 keV, the main process variables being the ion fluence (ranging from 3x10^15 cm^-2 to 3x10^17 cm^-2) and the final etching process (wet etch, H2 plasma and annealing in air). The substrates were characterized by atomic force microscopy, optical profilometry and white beam X-ray topography. The influence of the various process parameters on the resulting lift-off efficien"},"claims":{"count":0,"items":[],"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"source":{"id":"1608.07171","kind":"arxiv","version":1},"verdict":{"id":null,"model_set":{},"created_at":null,"strongest_claim":"","one_line_summary":"","pipeline_version":null,"weakest_assumption":"","pith_extraction_headline":""},"references":{"count":0,"sample":[],"resolved_work":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57","internal_anchors":0},"formal_canon":{"evidence_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"author_claims":{"count":0,"strong_count":0,"snapshot_sha256":"258153158e38e3291e3d48162225fcdb2d5a3ed65a07baac614ab91432fd4f57"},"builder_version":"pith-number-builder-2026-05-17-v1"}